Farida Ariani,Adhitasari Suratman,Dwi Siswanta
出处
期刊:Key Engineering Materials
日期:2023-07-26
卷期号:949: 57-65
被引量:2
摘要
In a batch system, The Cu(II) preconcentration parameters were optimized using chitosan-crosslinked dialdehyde carboxymethyl cellulose (CS-DCMC). The experiment was started with the oxidation of carboxymethyl cellulose by periodate to form DCMC. The CS-DCMC adsorbent was then prepared with a mass ratio of CS-DCMC=1:1. The adsorbent is characterized by FTIR for functional group analysis and SEM-EDX for morphological analysis and the percentage of elements in CS-DCMC adsorbent. In the optimization of preconcentration parameters, the optimal adsorption, desorption, and enrichment factors were obtained at pH 4, adsorbent mass of 90 mg, adsorption time of 95 min, Cu(II) concentrations of 7 mg/L, and Na 2 EDTA 1 M. The application of CS-DCMC on wastewater containing Cu(II) under optimal conditions gave good results. Wastewater containing Cu(II) 0.1 mg/L can be concentrated to 0.53 mg/L with an enrichment factor of 5.26 times, 0.2 mg/L Cu(II) can be concentrated to 1.08 mg/L with an enrichment factor of 5.40 times, and 0.3 mg/L Cu(II) can be concentrated to 1.68 mg/L with an enrichment factor of 5.59 times. The enrichment factor obtained is almost close to the theoretical enrichment factor of 6 times.
科研通智能强力驱动
Strongly Powered by AbleSci AI