A simple microemulsion-based method has been developed to synthesize ZnCo(2)(C(2)O(4))(3) nanowires that can be transformed to porous ZnCo(2)O(4) nanowires under annealing conditions. The morphology of porous ZnCo(2)O(4) nanowires can be tuned by the initial ZnCo(2)(C(2)O(4))(3) nanowires and the annealing temperatures. The as-synthesized porous ZnCo(2)O(4) nanowires have been applied as anode materials of Li-ion batteries, which show superior capacity and cycling performance. The porous one-dimensional (1D) nanostructures and large surface area are responsible for the superior performance. Moreover, it is indicated that porous ZnCo(2)O(4) nanowires synthesized at low annealing temperature (500 °C) show larger capacity and better cycling performance than that prepared at high annealing temperature (700 °C), because of their higher porosity and larger surface area.