红麻
材料科学
复合材料
抗弯强度
极限抗拉强度
硅烷
聚丙烯
氢氧化钠
纤维
化学
物理化学
作者
Oscar Asumani,R.G. Reid,R. Paskaramoorthy
标识
DOI:10.1016/j.compositesa.2012.04.007
摘要
Kenaf fibre reinforced polypropylene composites were manufactured by compression moulding. The kenaf fibre was considered in three forms; untreated, treated with sodium hydroxide solution and treated with sodium hydroxide solution followed by three-aminopropyltriethoxysilane. The effects of these chemical treatments on the tensile and flexural properties of the composites were investigated. Mechanical test results show that alkali treatment followed by three-aminopropyltriethoxysilane treatment (alkali–silane treatment) significantly improves the tensile and flexural properties of short fibre non-woven kenaf polypropylene composites. In particular, the specific tensile and flexural strengths of alkali–silane treated kenaf composites with 30% fibre mass fraction are, respectively, only 4% and 11% lower than those of composites made using glass fibre. Scanning electron microscopy examination shows that the improvements in the tensile and flexural properties resulting from alkali–silane treatment can be attributed to better bonding between the fibres and matrix.
科研通智能强力驱动
Strongly Powered by AbleSci AI