材料科学
钩子
焊接
接头(建筑物)
断裂(地质)
复合材料
剪切(地质)
点焊
极限抗拉强度
冶金
结构工程
工程类
作者
Tao Yuan,Shaoqian Kang,Xiaoqing Jiang,Fajie Tang,Yanjun Gao,Xing Zheng
标识
DOI:10.1080/02670836.2022.2093001
摘要
The mechanical properties and failure process of 2 mm-thick 5052 Al and 6 mm-thick 2A12 Al fabricated by refill friction stir spot-welding were investigated. The hooks were bent respectively downwards and upwards at plunge depths smaller and larger than the upper plate thickness. The joint area of the lap interface and bearing thickness of the upper plate were related to the hook direction. The tensile shear failure load was affected by structural characteristics and hardness of the joints. Stress concentration occurred in the hook and strain expanded with the hook during fracture. There were two fracture modes: shear fracture and shear plug fracture, where both cracks passed through the hook and fracture morphology of the hook was less plastic.
科研通智能强力驱动