The flexure of spherical rigid contact lenses was measured on the eyes of 10 young subjects using a videokeratoscope. Five subjects had little or no with-the-rule astigmatism (<0.75 D) andfive had moderate levels of with-the-rule astigmatism (1.00-2.00 D). Two lens materials (polymethylmethacrylate [PMMA] and Boston XO) in three centre thicknesses (0.05, 0.10 and 0.15 mm) were used in the study. No significant difference in the amount of flexure was found between the two materials tested. The degree of regular astigmatism on the lens front surface was found to increase as the centre thickness of the contact lens decreased. For the astigmatic group, the lenses with centre thicknesses of 0.05 mm had levels of front surface astigmatism similar to those of the underlying cornea. On spherical corneas the level of regular astigmatism can exceed that of the cornea for thinner lenses. When sphero-cylinder variations are accounted for, residual higher order aberration (root mean square) levels were found to approach those of the cornea when the lens thickness was reduced to 0.05 mm.
科研通智能强力驱动
Strongly Powered by AbleSci AI