Ying Xu,Peng Song,Weigang Cao,Hui Li,Jinglong Liang
出处
期刊:Crystals
[MDPI AG]
日期:2021-08-12
卷期号:11 (8): 936-936
被引量:6
标识
DOI:10.3390/cryst11080936
摘要
Steel slag, as industrial solid waste, is difficult to recycle owing to its complex components and poor mechanical properties. However, steel slag can be modified by adding Al2O3–SiO2 through high temperature sintering, which would improve the mechanical properties and expand the scope of its application. The phase changing, morphology evolution and the mechanical properties of the modified steel slag were investigated. The results indicate that the main phase changes to gehlenite occur with increasing temperature. The compressive strength increases to 115 MPa at 1350 °C. The relationship of the quantity of gehlenite and the compressive strength were explored.