Yao Ying,Jiawei Feng,Zhaocheng Li,Jingwu Zheng,Jing Yu,Wangchang Li,Liang Qiao,Wei Cai,Juan Li,Hui Huang,Tiejun Zhao,Shenglei Che
摘要
Abstract In this study, MnZn ferrites with added YIG nanoparticles were developed for MHz frequency applications. The effect of the magnetic YIG additive on the power loss, initial permeability, and cutoff frequency of MnZn ferrites was investigated. A small quantity of added YIG effectively reduces the power loss and concurrently increases the initial permeability. Compared to the results for the MnZn ferrite with no added YIG, the optimal MnZn ferrite with 600 ppm added YIG exhibits a reduction in the power loss at 25°C of 56.4% and 36.6% at 1 MHz/50 mT and 3 MHz/10 mT, respectively, and a 13.9% increase in the initial permeability. This sample also exhibits a good stability of the power loss against temperature. The power loss remains below 205 kW/m 3 over temperatures ranging from 25 to 140°C. The effect mechanism of YIG addition on the magnetic properties of MnZn ferrites was studied. An analysis based on the equivalent circuit model showed that the reduction in the eddy current loss and power loss mainly results from the increase in the grain boundary resistance caused by the addition of highly resistive YIG.
科研通智能强力驱动
Strongly Powered by AbleSci AI