材料科学
烧结
均质化(气候)
微观结构
透射率
陶瓷
透明陶瓷
复合材料
兴奋剂
光电子学
生物多样性
生态学
生物
作者
Dong Suk Kim,Jong Heun Lee,Rak Joo Sung,Sang Woo Kim,Hyung Soo Kim,Jeong Shik Park
标识
DOI:10.1016/j.jeurceramsoc.2007.02.002
摘要
Pure, 140, 500, and 2500 ppm MgO-doped Al2O3 specimens were sintered at 1700 °C in a vacuum with and without pre-sintering heat treatment (HT) at 800 °C for 50 h in air. Pre-sintering HT improved the transmittance in the visible (400–700 nm) range significantly. This enhanced transmittance was explained in terms of the removal of residual pores and the homogenization of the microstructure due to the lowering of the boundary mobility as a result of the MgO addition and the suppression of local densification through a pre-coarsening step.