搪瓷漆
臼齿
胶粘剂
材料科学
磷酸
复合数
粘结强度
蚀刻(微加工)
复合材料
牙科粘接
牙科
冶金
图层(电子)
医学
作者
Yu-Lynn Lee,Kai Chun Li,Cynthia Kar Yung Yiu,Dorothy Boyd,John Neil Waddell,Manikandan Ekambaram
出处
期刊:PubMed
日期:2021-12-03
卷期号:23 (6): 513-525
被引量:4
标识
DOI:10.3290/j.jad.b2288247
摘要
To investigate the effect of pretreatment protocols involving Papacarie Duo gel and Scotchbond Universal (SU) on the microshear bond strength (µSBS) of resin composite (RC) to hypomineralised enamel (HE).Specimens of normal enamel (NE) and HE were derived from extracted hypomineralised first permanent molars (FPMs). Based on the colour of demarcated opacities, HE specimens were classified as creamy/white (CW) or yellow/brown (YB). The specimens were randomly allocated into eight groups (n = 20). Each group involved pretreatment with Papacarie Duo gel or no pretreatment, and SU applied in etch-and-rinse (E&R) or self-etch (SE) mode. All specimens were bonded with RC and subjected to µSBS testing. Failure modes were analysed using an optical microscope and SEM.Comparing NE with HE, the following factors were found to be significant (p < 0.001): type of enamel substrate, deproteinising pretreatment, and etching mode. Comparing CW HE with YB HE, a significant interaction between "deproteinising pretreatment" and "etching mode" was demonstrated (p = 0.028). When subjected to the concurrent use of Papacarie Duo gel and phosphoric acid etching, HE specimens showed a significant increase in µSBS (p < 0.001).Deproteinising pretreatment using Papacarie Duo gel followed by the application of SU in E&R mode led to increased µSBS of resin composite to HE.
科研通智能强力驱动
Strongly Powered by AbleSci AI