曲轴
断口学
材料科学
圆角(机械)
卡车
猝灭(荧光)
断裂(地质)
复合材料
疲劳极限
疲劳试验
结构工程
弯矩
工程类
汽车工程
机械工程
荧光
物理
量子力学
作者
Yucheng Luo,Gao Yue,Biyang Chen,Bin Huang,Fei Liu,Lei Zhou,Xiaofeng Mao,Shigui Deng,Juan Du,Kunming Liu
标识
DOI:10.1016/j.engfailanal.2023.107724
摘要
A failure investigation was performed into the fractured 42CrMo4 crankshaft used for wide-body mining dump truck in this paper. Fracture morphology, chemical composition, microstructure and mechanical properties of the crankshaft material were studied to investigate the premature failure mechanism. All the crankshaft broke at the 4th or 6th necks and a high-cycle bending fatigue type in this case could be identified by the observation of beach marks and fatigue striations in the propagation area according to fractography results. The fatigue source is underneath the hardening layer of R fillet and the root cause could be identified as the designed inadequate thickness of quenching layer at the fillets obtained through medium frequency induction quenching (MFIQ), which could not provide adequate fatigue strength upon cyclic loadings for long term. Fatigue validation test indicated that the bending moment increased with the increasing thickness of the quenching layer, and the appropriate thickness was recommended about 3.5 mm based on overall consideration.
科研通智能强力驱动
Strongly Powered by AbleSci AI