摘要
Polymerization, and copolymerization with styrene, of m,p-chloromethylstyrene have been carried out at 75°C, in chlorobenzene and in the presence of AIBN ([AIBN] ⋍ 6 × 10−2, and 12 × 10−2m, respectively). The polymer molecular weights, determined by g.p.c., are: Mw = 8670, Mn = 5860, and Mw/-Mn = 1.48 for the homopolymer, poly(m,p-chloromethylstyrene), (1a); and Mw = 8805, Mn = 5144, and Mw/-Mn = 1.71 for the copolymer, copoly(m,p-chloromethylstyrene-styrene), (2a). A series of phosphine derivatives of both 1a and 2a are prepared by the reaction of the polymers with either chlorodiphenylphosphine/lithium, or diphenylphosphine/potassium tert. butoxide. A number of other potentially electroreactive derivatives of 2a are obtained by reacting the polymer with 2-aminoanthraquinone, 3-N-methylamino-propionitrile, or 2-(2-aminoethyl) pyridine. The phosphinated polymers are reacted with bis-benzonitrilepalladium-(II) chloride to obtain a series of polymer-palladium(II) complexes containing 8.5–12.9% palladium. Similarly, reaction of the last-named bidentate polymeric ligand with cupric acetylacetonate, or cupric sulphate pentahydrate, produces polymer-copper(II) complexes having 5.8, or 3.3% copper, respectively. The inter/intra-chain nature of some of the side reactions during the derivatization of the chloromethylated polymers, and that of the complex formation between transition metal centres and macromolecular ligands, are briefly discussed in view of the experimental results.