摘要
Occupational exposure to N-nitrosamines in the rubber industry was first reported by Fajen et al. (1979). In order to study the origin and formation of nitrosamines in this industry, chemicals and industrial products, as well as the air in various working areas, were analysed (Spiegelhalder et al., 1980). All chemicals used for rubber compounding contain nitrosamines if they are derivatives of secondary amines; e.g., tetramethylthiurame, zinc-diethyldithiocarbamate or N-oxydiethylene benzothiazolylsulfenamide. All rubber products containing these dialkyl amine derivatives exhibited considerable levels of the corresponding nitrosamines. Accordingly, variable concentrations of airborne nitrosamines could be detected at places where rubber products are manufactured or stored. The nitrosamines found correspond to the compounded chemicals. The original nitrosamine level in rubber chemicals is not high enough to explain the amounts found in rubber products and in air, so that additional nitrosation must occur. The responsible nitrosating agents are described. Preliminary results show that, in most cases, the elimination of nitrosating agents or the use of different rubber chemicals can drastically reduce nitrosamine levels in rubber products and in working areas.
科研通智能强力驱动
Strongly Powered by AbleSci AI