海泡石
纳米颗粒
电化学
材料科学
化学工程
纳米技术
钴
比表面积
纳米复合材料
介电谱
热重分析
共沉淀
作者
Wenwu Jiang,Yi Han,Yunhong Jiang,Fu Xu,Donghong Ouyang,Jinlei Sun,Ana C. S. Alcântara,Mercedes Suárez,Yanhuai Ding
标识
DOI:10.1016/j.clay.2021.106020
摘要
Abstract In this paper, Co3O4/sepiolite composites have been synthesized by using electrochemically active sepiolite as templates. The Co3O4/sepiolite composite delivered an initial discharge capacity around 1947 mAhg−1 at 1.0 Ag−1 with capacity retention up to 867 mAhg−1 after 1000 cycles. Besides, the composite released a high specific discharge capacity around 453 and 206 mAhg−1 at 5.0 and 15.0 Ag−1, respectively. A long-term activation process can be observed in the lithiation/delithiation reaction, which is beneficial to improve the cycling performance of Co3O4/sepiolite composites.
科研通智能强力驱动
Strongly Powered by AbleSci AI