微晶
材料科学
热稳定性
单晶
热失控
开裂
热的
图层(电子)
化学工程
电极
复合材料
阴极
结晶学
冶金
化学
热力学
物理化学
工程类
物理
功率(物理)
电池(电)
作者
Guilong Liu,Jianping Li,Naiteng Wu,Lu Cui,Xiaxiao Huang,Xianming Liu,Yunxia Zhao,Haipeng Chen,Weiwei Yuan,Yang Bai
出处
期刊:Journal of The Electrochemical Society
[The Electrochemical Society]
日期:2018-01-01
卷期号:165 (13): A3040-A3047
被引量:105
摘要
The fire incidents triggered by the thermal runaway of Li-ion batteries (LIBs) have aroused widespread concerns, as the instabilities of the delithiated cathode materials are generally accepted as one of the reasons for the ignition of LIBs. Herein, the electrochemical performance and the thermal stability of single-crystal and polycrystalline LiNi0.6Co0.2Mn0.2O2 electrode were investigated, trying to explore a novel, advanced approach for the thermal and cyclic stability of LiNi0.6Co0.2Mn0.2O2. Our results showed that the collapses of the layer structures and the cracks of polycrystalline particles occurred during charge; compared with the polycrystalline materials, the single-crystal particles efficiently improved the thermal stability, cyclic performance, and collapse of the layer structures. Additionally, the single-crystal material could maintain the structure and morphology even under a high charging voltage of 4.95 V. After 800 cycles at 45°C, 92.5% of the initial capacity was maintained for the single-crystal LiNi0.6Co0.2Mn0.2O2, while the capacity retention of the polycrystalline materials was below 90.5% after 300 cycles.
科研通智能强力驱动
Strongly Powered by AbleSci AI