摘要
In this study, polyurea was experimentally tested under various spraying temperatures and pressures. The number of holes and the pore size produced after the tensile fracture of the polyurea were counted to illustrate the effect of the various spraying temperatures and pressures on the performance of the polyurea. The tensile characteristics of polyurea were greatly influenced by the spraying temperatures and pressures, according to the experimental findings and statistical analysis. The polyurea tensile performance was best when the spraying pressure was 17.25 MPa with a spraying temperature of 70 °C. The fracture mechanism was illustrated by the silver streaking phenomenon generated during the tensile stretching process. The fracture energy was absorbed by the fracture holes and pores during silver streaking, thus creating the huge gap in tensile properties.
科研通智能强力驱动
Strongly Powered by AbleSci AI