期刊:Chemical Communications [The Royal Society of Chemistry] 日期:2021-01-01卷期号:57 (77): 9918-9921被引量:41
标识
DOI:10.1039/d1cc04337d
摘要
A primary battery with a high areal energy of 7.7 mW h cm −2 and a flat discharge plateau at around 0.7 V was developed by employing sulfur, Zn foil and 1 M ZnCl 2 aqueous solution as the cathode, anode and electrolyte, respectively.