Xinchun Tian,Geoffrey L. Brennecka,Xiaoli Tan
出处
期刊:ACS Nano
[American Chemical Society]
日期:2020-06-12
卷期号:14 (7): 8328-8334
被引量:4
标识
DOI:10.1021/acsnano.0c02346
摘要
One of the main challenges for next-generation electric power systems and electronics is to avoid premature dielectric breakdown in insulators and capacitors and to ensure reliable operations at higher electric fields and higher efficiencies. However, dielectric breakdown is a complex phenomenon and often involves many different processes simultaneously. Here we show distinctly different defect-related and intrinsic breakdown processes by studying individual, single-crystalline TiO2 nanoparticles using in situ transmission electron microscopy (TEM). As the applied electric field intensity rises, rutile-to-anatase phase transition, local amorphization/melting, and ablation are identified as the corresponding breakdown processes, the field intensity thresholds of which are found to be related to the position of the intensified field and the duration of the applied bias relative to the time of charged defects accumulation. Our observations reveal an intensity-dependent dielectric response of crystalline oxides at breakdown and suggest possible routes to suppress the initiation of premature dielectric breakdown. Hence, they will aid the design and development of next-generation robust and efficient solid dielectrics.
科研通智能强力驱动
Strongly Powered by AbleSci AI