摘要
ZnO is an important semiconductor that has been widely applied in solar cell, photocatalysis, environmental remediation. Doping and morphology control are important approaches to improve its photocatalytic performance. Herein, a facile two-step calcination method was developed to fabricate carbon(C)-doped cubic ZnO with porous structure from zeolite imidazolate frameworks (ZIF-8). Compared with one-step pyrolysis, the approach of two-step calcination not only retains the cubic morphology with inter-connected ZnO nanoparticles and porous structure but also introduces C doping in ZnO lattice effectively. This morphology has advantage in charge transfer, optical absorption and mass transfer during the photoreaction, and C doping results in high charge-separation efficiency. The sample C350-400 (C-doped ZnO, firstly calcined at 350 °C for 2 h from ZIF-8, then 400 °C for 1 h) shows the maximum photoactivity, which is ca. 3-fold and 4-fold higher than ZnO (C450) in photodegradation and PEC water splitting (under UV–vis irradiation), respectively. It is expected that the preparation of metal oxide from MOF is a very promising way to fabricate highly efficient photocatalyst.
科研通智能强力驱动
Strongly Powered by AbleSci AI